Ceadaíonn úsáid ferrovanadium:
friotaíocht teasa cruach a mhéadú;
neart tionchair agus friotaíocht faghartha na miotail a mhéadú;
cruach a dhéanamh láidir agus resistant a strus meicniúil;
hardenability cruach a mhéadú.
Ferrovanadium

Comhdhéanamh Ferrovanadium
| Branda | Ábhar, % | ||||||||
| Vanaidiam | Mangainéis | sileacain | Carbón | Copar | Arsanaic | Alúmanam | Fosfar | Sulfar | |
| ní mó | |||||||||
| FVd50U0.4 | 48-60 | 2.7 | 1.8 | 0.4 | 0.2 | 0. 01 | 0.2 | 0. 07 | 0. 02 |
| FVd50U0.5 | 48-60 | 4 | 2 | 0.5 | 0.2 | 0. 01 | 0.3 | 0. 07 | 0. 02 |
| FVd50U0.6 | 48-60 | 5 | 2 | 0.6 | 0.2 | 0. 02 | 0.3 | 0. 07 | 0. 03 |
| FVd50U0.3 | ó 50 | 0.2 | 2 | 0.3 | 0.2 | 0. 05 | 2.5 | 0.1 | 0.1 |
| FVd50U0.75 | ó 50 | 0.2 | 2 | 0.75 | 0.2 | 0. 05 | 2.5 | 0.1 | 0.1 |
| FVd40U0.5 | 35-48 | 2 | 2 | 0.5 | 0.4 | 0. 03 | 0.5 | 0. 08 | 0. 05 |
| FVd40U0.75 | 35-48 | 4 | 2 | 0.75 | 0.4 | 0. 03 | 0.5 | 0. 08 | 0. 05 |
| FVd40U1 | 35-48 | 6 | 2 | 1 | 0.4 | 0. 03 | 0.5 | 0.1 | 0. 05 |