Is cóimhiotal iarainn agus vanadium é Ferrovanadium a bhfuil cion vanadium ann ó 35% go 85%. Úsáidtear Ferrovanadium go príomha mar bhreiseán príomhúil i dtáirgeadh cruach le haghaidh comhlachtaí feithicleach, struchtúir tógála agus trealamh leighis.
Vanaidiam Ferro

Paraiméadair Ferrovanadium
| Grád | IN | Al | n | Si | LEIS |
| FeV40-A | 38-45 | 1.5 | 0.09 | 2 | 0.6 |
| FeV40-B | 38-45 | 2 | 0.15 | 3 | 0.8 |
| FeV50-A | 48-55 | 1.5 | 0.07 | 2 | 0.4 |
| FeV50-B | 45-55 | 2 | 0.1 | 2.5 | 0.6 |
| FeV60-A | 58.0~65.0 | 1.5 | 0.06 | 2 | 0.4 |
| FeV60-B | 58.0~65.0 | 2 | 0.1 | 2.5 | 0.6 |
| FeV60-A | 58.0~65.0 | 0.4 | 2 | 0.06 | 0.04 |
| FeV60-B | 58.0~65.0 | 0.6 | 2.5 | 0.1 | 0.05 |
| FeV80-A | 78-82 | 1.5 | 0.05 | 1.5 | 0.15 |
| FeV80-B | 78-82 | 2 | 0.06 | 1.5 | 0.2 |
Is branda uathúil muid sa mhargadh a thairgeann raon eisiach táirgí miotalóireachta dár gcliaint a bhfuil meas orthu.