Whatever your specific requirements, whether it's low-carbon ferrosilicon 65 for high-precision steel production, our five main grades cover the full range of industrial needs. Our state-of-the-art 30,000-square-meter factory is equipped with everything you need to manufacture products to your exact specifications, as well as rigorous internal testing to ensure compliance with international standards such as ASTM and ISO .
![]()
Sonraíocht FESI65 Ferro Silicon Alloy Lumps
|
Grád |
Níos mó ná nó cothrom le |
(Comhdhéanamh ceimiceach) níos lú ná nó cothrom le % |
||||||
|
|
SI |
Bal de |
Caoiseach |
MN |
Cc |
P |
S |
C |
|
FESI75 |
75 |
1.5 |
1 |
0.5 |
0.5 |
0.04 |
0.02 |
0.2 |
|
FESI72 |
72 |
2 |
1 |
0.5 |
0.5 |
0.04 |
0.02 |
0.2 |
|
FESI70 |
70 |
2 |
1 |
0.6 |
0.5 |
0.04 |
0.02 |
0.2 |
|
FESI65 |
65 |
2 |
1 |
0.8 |
0.5 |
0.04 |
0.02 |
0.2 |
|
FESI45 |
45-47 |
2 |
1 |
0.8 |
0.5 |
0.04 |
0.02 |
0.2 |
Ár Monarcha
![]()
Cuairt custaiméirí
![]()
Ceisteanna CCanna
C: An féidir leat na fadhbanna a réiteach maidir le do tháirgí a úsáid?
A: Tá . Tá taithí charntha ag ár gcuideachta le fada, is féidir leis na fadhbanna go léir sa phróiseas úsáide a réiteach .
C: An bhfuil aon taithí agat ar tharaifí nó ar chostais d'onnmhairí a laghdú?
A: Tá foireann ghairmiúil ag ár gcuideachta chun costais do chustaiméirí a laghdú .
An féidir liom samplaí a fháil?
Is féidir, is féidir in iolraithe coimeádáin / vaigín / eurofour . trí réamhíocaíocht ón gceannaitheoir .
An féidir liom mo tháirge saincheaptha féin a bheith agam?
Sea, déanaimid é a phlé ina n -aonar .
Cá fhad a thógann sé an costas loingseoireachta a ríomh?
{12-48 uair an chloig .
An dtugann tú lascaine ag brath ar chainníocht an ordaithe?
Cuirimid ar fáil ón toirt don loingsiú farraige, conradh bliantúil .
Clibeanna Te: FESI65 Ferro Silicon Alloy Lumps, an tSín FESI65 Ferro Silicon Alloy Déantóirí, Soláthraithe